Mechanical Properties Metric English Comments
Tensile Stress 35.0 MPa
5080 psi
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 35.0 MPa
5080 psi
Lehmann & Voss LUVOCOM® 1850-7692 PBT, with glass spheres and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Tensile Stress 35.0 MPa
5080 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene
EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a..
Tensile Stress 35.0 MPa
5080 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene
EX4 is a high density polyethylene with 1-Butene as co monomer. It is high rigidity, low gel level, high drowdown, somewhat stiffer than EX 5.Applications: film extrusion, blending partner, refuse ..
Tensile Stress 35.0 MPa
5080 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene
EX5 is a high density polyethylene with 1-Butene as co monomer.Applications: film extrusion, counter bag, carrier bag, wrapping filmsInformation provided by Iran Petrochemical Commercial Co.
Tensile Stress 35.0 MPa
5080 psi
ISO R527
Iran Petrochemical (PCC) Moplen Z 30 S Polypropylene
Moplen Z 30S is a high melt flow homopolymer for the production of low denier BCF, CF, and staple fibers at medium to high spinning speeds. Moplen Z30S offers a high homogeneity, stable extrusion a..
Tensile Stress 35.0 MPa
5080 psi
at Break; ISO 527
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene
EX 4HS is a high density polyethylene with 1-Butene as co monomer. It has high rigidity, low gel level, high drawdown, very high stiffness and good tenacity.Applications: film extrusion, blending ..
Tensile Stress 35.0 MPa
5080 psi
ISO R527
Iran Petrochemical (PCC) S 28 F Polypropylene Film
Biaxially oriented poly propylene films suitable for metallization Applications: cosmetics , food stuffs , lamination and other flexible films.Information provided by Iran Petrochemical Commercial C..
Tensile Stress 35.0 MPa
5080 psi
ISO R527
Iran Petrochemical (PCC) S 30 G Polypropylene
The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Pe..
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
5080 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
Tensile Stress 35.0 MPa

@Strain 50.0 %
5080 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® AZ 3/2 PA66
Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE..