Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
PolyOne Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
PolyOne Edgetek® LC-30GF/000 LCP (Liquid Crystal Polymer), 30% Glass Reinforced, Hi-Temp
(discontinued **)< Information provided by PolyOne™ Corporation |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated
(disco Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1850-7784 PBT, with glass fiber, glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-8286 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | |
Kuraray Genestarâ„¢ TA104 Nylon Reinforced injection grade.Main Features:High reflectivityLess color change by heat and lightHigh reliabilityExample of applications:LED reflectors |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | |
Sylvin Technologies 8999-95 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP DX10313 PC (Asia Pacific) DX10313 is high modulus polycarbonate, 50% glass filled, with balanced flow and impact strength |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Samyang Tripet® 2550GN30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White HS8350 Concentrate Based In Impact Polystyrene DescriptionPOLYBATCH® HS8350 is a white masterbatch containing 50% TiO2 based in impact polystyrene. This product has been formulated to optimize the dispersion and opacity with good distributive .. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Grey 8368 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8368 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall H 5177B Plenum Flexible PVC Plenum-grade jacket with good low temperature properties for use over 100% FEP primaries. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
Specific Gravity | 1.61 - 1.65 g/cc | 1.61 - 1.65 g/cc | ASTM D-792 |
Axiall 1275 Plenum Flexible PVC Plenum-grade optical fiber jacket. UL QMTM2 recognized component for plenum cable compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | Method A; ASTM D792 |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Specific Gravity | 1.61 g/cc | 1.61 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ PI-30GF/15T Polyetherimide (PEI), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |