Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 80.0 °C @Time 21600 - 28800 sec |
176 °F @Time 6.00 - 8.00 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 28800 sec |
176 °F @Time 6.00 - 8.00 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 1850-7783-1 PBT, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 28800 sec |
176 °F @Time 6.00 - 8.00 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 1850-7784 PBT, with glass fiber, glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 28800 sec |
176 °F @Time 6.00 - 8.00 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 1850-7853 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 28800 sec |
176 °F @Time 6.00 - 8.00 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 1850-7942 PBT, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7277 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 28800 sec |
176 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7330 Polyamide 46, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Reduced moment of inertia compared with metal parts.Highly dimensionally stable at elevated tem.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7652 Polyamide 46, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Reduced moment of inertia comp.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 28800 sec |
176 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 19-7669 Polyamide 46, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7744 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7827 Polyamide 46, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-7969 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-8043 Polyamide 46, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 43200 sec |
176 °F @Time 2.00 - 12.0 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 28800 sec |
176 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Drying Temperature | 80.0 °C @Time 57600 sec |
176 °F @Time 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 20/AF/15/TF/10 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 57600 sec |
176 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Drying Temperature | 80.0 °C @Time 57600 sec |
176 °F @Time 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Drying Temperature | 80.0 °C @Time 57600 sec |
176 °F @Time 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Drying Temperature | 80.0 °C @Time 57600 sec |
176 °F @Time 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 20-8254 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Drying Temperature | 80.0 °C @Time 57600 sec |
176 °F @Time 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 20-8368 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 57600 sec |
176 °F @Time 6.00 - 16.0 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 21-7976 Polyamide 6/6T, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Drying Temperature | 80.0 °C @Time 601 sec |
176 °F @Time 0.167 hour |
|
Gwent Electronic Materials C2000215D4 Silver / Silver Chloride Paste C2000215D4 has a ratio of Silver to Silver Chloride of 50/50. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |
|||
Drying Temperature | 80.0 °C @Time 21600 - 28800 sec |
176 °F @Time 6.00 - 8.00 hour |
Vacuum Dryer |
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Drying Temperature | 80.0 °C @Time 7200 - 28800 sec |
176 °F @Time 2.00 - 8.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te.. |