Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Norton® Chemfilm® DF110 Fluoropolymer Cast Film

Category Polymer , Film , Thermoplastic , Fluoropolymer
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton® Chemfilm®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Norton® Chemfilm® DF110 Fluoropolymer Cast Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Used for Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D-792
Water Absorption <= 0.010 %
<= 0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.6 MPa
4300 psi
ASTM D-882
Elongation at Break 400 %
400 %
ASTM D-882
Tensile Modulus 0.414 GPa
60.0 ksi
ASTM D-882
Thermal Properties Metric English Comments
Melting Point 327 °C
620 °F
ASTM D-3418
Maximum Service Temperature, Air 260 °C
500 °F
UL-746 B
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistivity per Square 2.00e+17 ohm
2.00e+17 ohm
ASTM D-257
Dielectric Constant 2.0

@Frequency 1000 Hz
2.0

@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Users viewing this material also viewed the following: