Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ASTM D2240
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D412
Tensile Strength, Yield 5.00 MPa
725 psi
50% Elongation; ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D790
Resilience 30
30
% Bayshore Resilience; ASTM D2632
Tear Strength 90.0 kN/m
514 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 65
65
H-18 Wheel, 1000 g load, ASTM D3489
Thermal Properties Metric English Comments
Vicat Softening Point 49.0 °C
120 °F
Rate A; ASTM D1525
Glass Transition Temp, Tg -20.0 °C
-4.00 °F
DMA