Processing Properties Metric English Comments
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Plastcom SLOVAMID 66 T 15 MI PA66, 15% mineral filling
FeaturesPA 66 with the content of 15 % chemically modified mineral filling and impact modified. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produc..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Hostaform® MR130ACS POM, Specialty  (Unverified Data**)
Hostaform® acetal copolymer grade MR130ACS is a general purpose acetal with improved acid stabilization. Hostaform® MR130ACS demonstrates improved performance over standard acetals after intermit..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Hostaform® MT24U01 POM, Medical Technology  (Unverified Data**)
Hostaform® MT24U01 is a special grade developed for medical industry applications containing low residual monomers and no animal products. Hostaform® MT24U01 is a low melt viscosity for fast cycli..
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
DuPont Performance Polymers Zytel® LM70G35HSLX BK314 Nylon 66  (Unverified Data**)
Zytel® LM70G35HSLX is a 35% glass fiber reinforced, heat stabilized, lubricated polyamide 66 for injection molding. It is well suited for laser marking.Information provided by DuPont Performance Po..
Mold Temperature 70.0 - 120 °C
158 - 248 °F
DAM
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2/BK PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Lehmann & Voss LUVOCOM® 1850-7315 PBT, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Lehmann & Voss LUVOCOM® 1850-7783 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BFG30-FN00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
ISO 294
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Recommended
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Lehmann & Voss LUVOCOM® 1-0889-5 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically ..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® PC-50/GF/30/TF/15/ BK Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lanxess Durethan® ECO BV 30 H2 900500 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled materialInformation provided by LANXESS.
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..
Mold Temperature 100 - 120 °C
212 - 248 °F
actual surface temp
Unitika C300VN
Characteristics: Flame resistant, transparent (flame resistance: UL94 V0, 0.8 mm) High flowInformation provided by Unitika Ltd.
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Covestro Makrolon® 1804 Polycarbonate
MVR (300 °C/1.2 kg) 6.0 cm3/10 minhigh viscosityUV stabilizedoptimized for low plate-outimproved flammabilityUL 94 V-2/1.5 mm and 3.0 mmavailable in transparenttranslucent and opaque colorssolid sh..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Covestro Makrolon® 2806 Polycarbonate
ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran..
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Eurotec® Tecopet® PT70 GR20 NL100 PR PET, 20% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
Mold Temperature 60.0 - 120 °C
140 - 248 °F
80 - 90°C is recommended
Azoty Tarnow™ Tarnamid® T-27 CF40 Polyamide 6 40% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Mold Temperature 60.0 - 120 °C
140 - 248 °F
BASF Ultraform® S1320 003 POM
Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Thermx® CG933 BK010 PCT
Thermx® CG933 BK010 is a 30% glass reinforced, flame retardant, black polycyclohexylenedimethylene terephthalate resin for injection molding.Celenese acquired the Thermx product line from DuPont in..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese VECTRA® 1310MT 30% Glass Filled, Medical Grade Liquid Crystal Polymer (LCP)
Description: 30% glass reinforced Vectra grade designed for use in medical devices resistant to radiation and steam sterilization. Has established Drug and Device Master Files, and is USP Class VI c..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Celanese Hostaform® C 9021 GV3/20 POM, 20% Glass Reinforced  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade, reinforced with ca. 20 % glass spheresInformation provided by Celanese
Mold Temperature 60.0 - 120 °C
140 - 248 °F
Azoty Tarnow™ TARNOFORM 300 DW POM
Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding.Infor..
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, ..
Mold Temperature 80.0 - 120 °C
176 - 248 °F
Lehmann & Voss LUVOCOM® 50/GF/20/TF/10/BK Polycarbonate, with glass fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Mold Temperature 40.0 - 120 °C
104 - 248 °F
suitable temperature 60-80°C
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled
Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..