Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene 8000 TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.Key Features: Non-hygroscopic product, requires little to no drying before processing.Neutral, easy coloring formulation.Recommended for applications requiring excellent ozone resistance.Used in sealing applications.Recommended for applications requiring excellent flex fatigue resistance. UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification.EU and China RoHS compliant.Applications:General PurposeUses:Appliance ComponentsCell PhonesFlexible GripsKitchenware Stationary SuppliesStrain ReliefsProcessing Method: Blow Molding, Coextrusion, Extrusion, Extrusion Blow Molding, Injection Blow Molding, Injection Molding, Multi Injection Molding, Profile Extrusion, Sheet Extrusion, Thermoforming and Vacuum FormingAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
23°C; ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
2 mm, 15 sec; ISO 868
97
97
Air at 302°F, 168 hr; ASTM D573
Tensile Strength at Break 13.0 MPa
1890 psi
Across Flow; ASTM D412
13.2 MPa
1910 psi
Air at 302°F, 168 hr; ASTM D573
Tensile Stress 7.10 MPa

@Strain 100 %
1030 psi

@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 527 %
527 %
Air at 302°F, 168 hr; ASTM D573
620 %
620 %
Across Flow; ASTM D412
Tear Strength 48.0 kN/m
274 pli
73°C, Die C; ASTM D624
Compression Set 52 %
52 %
158°F, 22 hr; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
UL RTI, Electrical 100 °C
212 °F
UL 746
UL RTI, Mechanical with Impact 90.0 °C

@Thickness 1.10 mm
194 °F

@Thickness 0.0433 in
UL 746
95.0 °C

@Thickness 1.60 mm
203 °F

@Thickness 0.0630 in
UL 746
95.0 °C

@Thickness 3.00 mm
203 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 HB

@Thickness 1.10 mm
HB

@Thickness 0.0433 in
HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Processing Properties Metric English Comments
Processing Temperature 175 - 230 °C
347 - 446 °F
Rear Barrel Temperature 191 - 204 °C
375 - 400 °F
Middle Barrel Temperature 196 - 210 °C
385 - 410 °F
Front Barrel Temperature 196 - 210 °C
385 - 410 °F
Nozzle Temperature 210 - 221 °C
410 - 430 °F
Die Temperature 196 - 224 °C
385 - 435 °F
Extrusion
Melt Temperature 199 - 216 °C
390 - 420 °F
Processing
196 - 224 °C
385 - 435 °F
Extrusion
Mold Temperature 23.9 - 51.7 °C
75.0 - 125 °F
Processing
Moisture Content 0.080 %
0.080 %
Back Pressure 0.345 - 0.689 MPa
50.0 - 100 psi
Clamp Pressure 41.4 - 68.9 MPa
6000 - 10000 psi
Vent Depth 0.00254 cm
0.00100 in
Cushion 0.317 - 0.635 cm
0.125 - 0.250 in
Screw Speed 100 - 200 rpm
100 - 200 rpm
Descriptive Properties Value Comments
Change in Mass in Air -7.0%
150°C, 168 hr, ASTM D573
Color Natural Color
Form Pellets
Injection Rate Fast
Maximum Regrind % 20
Screw Compression Ratio 2:1 - 2.5:1
Screw L/D Ratio 16:1 - 20:1
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved