Thermal Properties Metric English Comments
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
ExxonMobil Santoprene® 121-85M100 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult ..
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer
A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w..
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746; ISO 812
Advanced Polymer Alloys Alcryn® 3055 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -53.9 °C
-65.0 °F
ASTM D746
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..