Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.10 MPa @Strain 100 % |
1030 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Tensile Stress | 7.10 MPa @Strain 100 % |
1030 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Tensile Stress | 7.10 MPa @Strain 100 % |
1030 psi @Strain 100 % |
Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tensile Stress | 7.10 MPa @Strain 100 % |
1030 psi @Strain 100 % |
ASTM D412 |
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |