Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 37.8 °C | 75.0 - 100 °F | |
RheTech Products FRG220-773UB 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Flame Retardant, UV Stabilized, Light Grey Applications: Electrical housingsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP102-00 Polypropylene, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 35.0 °C | 75.0 - 95.0 °F | |
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified .. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 9100-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 9100-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
RTP Company RTP 2099 X 115382 C Bio-Based Polylactic Acid (PLA); PLA-HDPE Blend - 39% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Mold Temperature | 23.9 - 60.0 °C | 75.0 - 140 °F | |
RTP Company RTP 2099 X 127618 R Bio-Based Polylactic Acid (PLA); PC-PLA Blend - Flame Retardant - Halogen Free - 20% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | For insertion injection molding |
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer A soft, black, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS b.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | Processing |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Mold Temperature | 23.9 - 51.7 °C | 75.0 - 125 °F | |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |
|||
Mold Temperature | 23.9 - 71.1 °C | 75.0 - 160 °F | |
RTP Company RTP 2099 X 121241 B Bio-Based Polylactic Acid (PLA); PC-PLA Blend - ESD Protection - Permanently Anti-static - 26% Renewable Resource Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |
|||
Mold Temperature | 23.9 - 71.1 °C | 75.0 - 160 °F | |
RTP Company RTP 2099 X 126210 BLACK Bio-Based Polylactic Acid (PLA); PC-PLA Blend - 32% Renewable Resource Content - Additional 49% Post Consumer Content For detailed processing information, see the PLA Molding Guide on the RTP Company website. |