Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 196 °C | 385 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by .. |
|||
Die Temperature | 196 - 224 °C | 385 - 435 °F | Extrusion |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Die Temperature | 196 °C | 385 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E.. |