Processing Properties | Metric | English | Comments |
---|---|---|---|
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9101-75 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Cushion | <= 0.317 cm | <= 0.125 in | Injection Molding |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Cushion | <= 0.317 cm | <= 0.125 in | Injection Molding |
Ineos ABS Lustran® ABS 349 Lustran® ABS 349 is a high-gloss, medium-impact injection molding resin that has been specially formulated for excellent surface lubricity using internal additives. |
|||
Cushion | <= 0.317 cm | <= 0.125 in | Injection Molding |
Ineos ABS Lustran® SAN DN59 SAN, Soft-Flow Grade Lustran® SAN DN59 resin is a soft-flow grade of transparent SAN (styrene acrylonitrile) thermoplastic. It has been designed for use in compounding and thin-wall injection molded applications. Lus.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 251-92W232 Thermoplastic Elastomer A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 171-55 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9201-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9201-65 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 241-45 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water. This grade .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 101-73 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |