Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 171 - 210 °C | 340 - 410 °F | |
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex.. |
|||
Front Barrel Temperature | 171 - 210 °C | 340 - 410 °F | |
PolyOne Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Overmold Adhesion to Polypro.. |
|||
Front Barrel Temperature | 177 - 210 °C | 351 - 410 °F | |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
Oxford Polymers C-Acetal -30GF-Natural Acetal Copolymer, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), Co-polymer Acetal, Injection Molding Grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass FiberSpecial Characteristic.. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP1-[color]-H Acetal Homopolymer, Low Flow, High Melt Strength, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources AH-GP2 Acetal Homopolymer, Medium Flow, Heat Stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 182 - 210 °C | 360 - 410 °F | |
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Front Barrel Temperature | 200 - 210 °C | 392 - 410 °F | |
Huntsman AVALON® 85 ABR Thermoplastic Polyurethane Introduction: AVALON 85 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical ALPHALAC SG910 HIPS High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA.. |
|||
Front Barrel Temperature | 200 - 210 °C | 392 - 410 °F | Injection Molding |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 200 - 210 °C | 392 - 410 °F | Injection Molding |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical 95HCTC SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Lighter, Cosmetic Container, ToothbrushCAS No. 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion |
Teknor Apex Sarlink® 3450 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion |
Teknor Apex Sarlink® 4145 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4145 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Front Barrel Temperature | 177 - 210 °C | 350 - 410 °F | Injection Molding |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Borealis Borcoat™ HE3450 Black High Density Polyethylene Top Coat for Steel Pipe Coating Borcoat HE3450 is a black, high-density polyethylene (HDPE) produced with the advanced Borstar technology, providing the material with especially well melt strength and extrudability. Also its mech.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Unitika TERRAMAC TE-8210 Polylactic Acid (PLA) High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion |
Teknor Apex Sarlink® 3490 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
Front Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion |
Teknor Apex Sarlink® 3439DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |