Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.940 - 0.960 g/cc
0.940 - 0.960 g/cc
ASTM D792
S&E Specialty Polymers GPP™ 1005M-EXLT PP
Application: UL94 V-2, Non-blooming flame retardant polypropylene compound for injection molding.Information provided by S&E Specialty Polymers
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet)
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
RTP Company RTP 6091-70A BLACK Specialty Thermoplastic Elastomer, PA-6 bondable - manufactured with Santoprene™ TPV technology
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Specific Gravity 0.940 - 0.960 g/cc
0.940 - 0.960 g/cc
Michelman® Coating X300™ Plus Water based, moisture and water resistant coating
Description: Water based, moisture and water resistant coating.Usage: Coating X300â„¢ Plus provides high levels of water resistance and good moisture resistance for kraft paper with improved wate..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Kraton® D1101 A (SBS) Liner Block Copolymer
Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Kraton® D1101 E (SBS) Liner Block Copolymer
Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D4025
Kraton® D1124 K (SIS) Radial Triblock Copolymer
Description: Kraton D1124 K is a clear, radial triblock copolymer based on styrene and isoprene, with a polystyrene content of 30%. It is supplied from North America in the physical form identified:..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Kraton® D1184 E (SBS) Branched Block Copolymer
Description: Kraton D1184 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Kraton® D1186 A (SBS) Branched Block Copolymer
Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Kraton® D1189 E (SBS) Radial Block Copolymer
Description: Kraton D1189 E is a clear, radial block copolymer based on styrene and butadiene with bound styrene of 32% mass. It is supplied from Europe in the physical forms indicated in the grade ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
A. Schulman LP552-01 Injection Molding, Extrusion Grade Compound
DescriptionLP 522-01 is an injection molding and/or extrusion grade compoundApplicationLP 552-01 meets FDA Regulation CFT 177.1520(c)3.1.Information provided by A. Schulman.
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
Zylog Neoplast® 155 FT SWB Thermoplastic Vulcanizate
Neoplast 155 FT SWB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant,..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate
DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer
DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and ..
Specific Gravity 0.940 g/cc
0.940 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 181-57W180 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It has USP Class VI Certificate of Compliance for biocompatibility, MEM elution cytotoxicity to ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer
Hot melt adhesive
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2782
AlphaGary Evoprene™ GC 5652 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
E-Polymers EFLEX® V1050 EPDM/TPV
V-series (Thermoplastic Vulcanizate Resins): E-FLEX V series resins are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic eq..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Specific Gravity 0.940 g/cc
0.940 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..