Polymer Property : Specific Gravity = 0.940 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Polimeri Europa Europrene® SOL T 6302 Styrene - Butadiene Block Copolymer
Europrene® SOL T 6302 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet)
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Quadrant EPP TIVAR® CleanStat™ FDA, USDA, 3-A Dairy, Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet)
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet)
Specific Gravity 0.940 g/cc
0.940 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Specific Gravity 0.940 g/cc
0.940 g/cc
LG Chemical SBR 1502 High Acrylonitrile Polymer
Description: SBR 1502 is a cold polymerized styrene-butadiene copolymer with styrene content of 23.5%. SBR 1502, a general purpose SBR, exhibits the excellent tensile strength, abrasion resistance,..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Kraton® D1152 E (SBS) Liner Block Copolymer
Description: Kraton D1152 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D412
Kraton® D1184 K (SBS) Branched Triblock Copolymer
Description: Kraton D1184 K is a clear, branched triblock copolymer based on styrene and butadiene, with a polystyrene content of 31%. It is supplied from North America in the physical form indentif..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Kraton® D4153 E (O/E SBS) Linear Block Copolymer
Description: Kraton D4153 E is an oil-extended linear block copolymer based on styrene and butadiene with bound styrene in the neat polymer of 35% mass. It contains 40 phr paraffinic oil which is cl..
Specific Gravity 0.940 g/cc
0.940 g/cc
Kraton® D4270 J (O/E SBS) Branched Block Copolymer
Description: Kraton D4270 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene in the neat polymer of 32% mass. It is supplied from Japan in the physical ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Kuraray SEPTON® H5125
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 55-HR-9 TPE
Product Description: StarTUFF TF 55-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..
Specific Gravity 0.940 g/cc
0.940 g/cc
Teknor Apex Tekbond® TB 2020A Thermoplastic Elastomer
Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Teknor Apex Telcar® OBC 2419C Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Teknor Apex Telcar® TL-355 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
A. Schulman POLYBATCH™ AC-20531L UV Absorber Concentrate
DescriptionPOLYBATCH® AC-20531L is a UV absorber concentrate containing 20% active additive based in low density polyethylene. POLYBATCH® AC-20531L is designed for use in polyethylene blown and c..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate
Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, ..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
A. Schulman FORMION™ FI 395 Ionomer
Information provided by A. Schulman.
Specific Gravity 0.940 g/cc

@Temperature 25.0 °C
0.940 g/cc

@Temperature 77.0 °F
Dow Corning ST Elastomer 10
A blend of a unique silicone elastomer and a volatile silicone fluid for use in a wide range of skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning
Specific Gravity 0.940 g/cc
0.940 g/cc
Part B
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy
Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe..
Specific Gravity 0.940 g/cc
0.940 g/cc
ATG s.r.l. BR Polybutadiene Rubber
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D471; ISO 2781
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCEHT Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6040NCEHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with improved surface..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Polimeri Europa Europrene® SOL T 161B Styrene - Butadiene Block Copolymer
Europrene® SOL T 161B is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 30% weight. A non-staining antioxidant ..
Specific Gravity 0.940 g/cc
0.940 g/cc
DIN-53479
Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry
Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops proper..
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183
Solvay Engineered Polymers DEXFLEX® 980HF TPO  (discontinued **)
Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
LyondellBasell DEXFLEX® 711 TPO
Description: DEXFLEX® 711 is a thermoplastic olefinic elastomer compounded with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched..
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792 and ISO 1183
ExxonMobil Santoprene® 8291-60B500 Thermoplastic Vulcanizate  (discontinued **)
Product Description: A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA 6, PA 6/6, PA 6 GF, PA 11, P..