Processing Properties | Metric | English | Comments |
---|---|---|---|
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8221-70 Thermoplastic Elastomer A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 241-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 271-73 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |