Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.710 mm |
203 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**) Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 1.50 mm |
203 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.750 mm |
203 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness >=0.710 mm |
203 °F @Thickness >=0.0280 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness >=1.50 mm |
203 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness >=3.00 mm |
203 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N109LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness >=1.50 mm |
203 °F @Thickness >=0.0591 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness >=3.00 mm |
203 °F @Thickness >=0.118 in |
|
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.810 mm |
203 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 171-64 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 1.50 mm |
203 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 76.2 mm |
203 °F @Thickness 3.00 in |
UL 746 |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 1.60 mm |
203 °F @Thickness 0.0630 in |
UL 746 |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.750 mm |
203 °F @Thickness 0.0295 in |
|
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.710 mm |
203 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 1.50 mm |
203 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 3.00 mm |
203 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.750 mm |
203 °F @Thickness 0.0295 in |
UL746B |
DSM Arnite® T08 200 (extrusion) T08 200 PBT (European and Asian Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 76.2 mm |
203 °F @Thickness 3.00 in |
UL 746 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 76.2 mm |
203 °F @Thickness 3.00 in |
UL 746 |
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.710 mm |
203 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |
|||
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 1.50 mm |
203 °F @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |