Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=1.50 mm |
194 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN2301F PC+GF30%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF30%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.60 mm |
194 °F @Thickness 0.0630 in |
UL 746 |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 27.9 mm |
194 °F @Thickness 1.10 in |
UL 746 |
ExxonMobil Santoprene® 8201-70 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.10 mm |
194 °F @Thickness 0.0433 in |
UL 746 |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 1.50 mm |
194 °F @Thickness 0.0591 in |
UL 746 |
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 0.750 mm |
194 °F @Thickness 0.0295 in |
UL 746B |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 38.1 mm |
194 °F @Thickness 1.50 in |
UL 746 |
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for.. |
|||
UL RTI, Mechanical with Impact | 90.0 °C @Thickness 38.1 mm |
194 °F @Thickness 1.50 in |
UL 746 |
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |