Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurostar Star L PA6 D61 PA6, Injection Molded

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer Eurostar Engineering Plastics
Trade Name Star L
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurostar Star L PA6 D61 PA6, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm

@Thickness 4.00 mm
0.018 - 0.022 in/in

@Thickness 0.157 in
E2P method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 62.0 MPa
8990 psi
ISO 527
Elongation at Break 18 %
18 %
ISO 527
Flexural Strength 79.0 MPa
11500 psi
ISO 178
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80x10x4; ISO 180/1A
Izod Impact, Unnotched (ISO) 68.0 kJ/m²
32.4 ft-lb/in²
80x10x4; ISO 180/1U
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Flatw 80x10x4, sp=64 mm; ISO 75/Af
Processing Properties Metric English Comments
Zone 1 230 - 240 °C
446 - 464 °F
Zone 2 235 - 245 °C
455 - 473 °F
Zone 3 240 - 260 °C
464 - 500 °F
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 75.0 - 85.0 °C

@Time 14400 - 21600 sec
167 - 185 °F

@Time 4.00 - 6.00 hour
Moisture Content 0.20 %
0.20 %
Copyright © lookpolymers.com All Rights Reserved