Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 1 = 230 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 3300-2LM PBT, Glass Reinforced  (Unverified Data**)
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release.30% glass-filled PBT, laser markableInfo..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 4202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.15% glass-fiber, improved impactInformation provided by Celanese
Zone 1 230 - 260 °C
446 - 500 °F
hopper
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,..
Zone 1 230 - 260 °C
446 - 500 °F
hopper
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
Zone 1 230 - 250 °C
446 - 482 °F
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh..
Zone 1 230 - 250 °C
446 - 482 °F
Lehmann & Voss LUVOCOM® 6-8436 Polyamide 12, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion.Isotropic shrinkage characteristics.Bearings, sleeve..
Zone 1 230 - 245 °C
446 - 473 °F
Extrusion Molding
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE.
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethanol for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Hydrochloric Acid (10%) for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 - 240 °C
446 - 464 °F
Eurostar Star L PA D51 PA6, Injection Molded
Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 1 230 - 240 °C
446 - 464 °F
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded
Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Zone 1 230 - 240 °C
446 - 464 °F
Eurostar Staramide PF006S PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF006S is a 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 1 230 - 240 °C
446 - 464 °F
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 1 230 - 240 °C
446 - 464 °F
Celanese CELANEX 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese
Zone 1 230 - 240 °C
446 - 464 °F
Celanese CELANEX 3100-2 PBT, 7.5% Glass Reinforced
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.Information ..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese CELANEX 3300-2 PBT, 30% Glass Reinforced
Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 1662Z PBT, 30% Glass Reinforced
Celanex 1662Z is a 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processabilityTo avoid hydrolytic degradation during processing, CELANEX resins ha..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 4302HS PBT, 30% Glass Reinforced
Celanex 4302HS is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance. Celanex 4302HS is ideally suited for heat shock applications such as ignition co..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 5214HF PBT, 15% Glass Reinforced
Celanex 5214HF is a high flow, 15% glass reinforced, high gloss, flame retardant polyester.Pre-drying: 250F (120C) for 4 HoursInformation provided by Celanese Corporation.
Zone 1 230 - 240 °C
446 - 464 °F
Celanese VANDAR 4602Z PBT, Unfilled
4602Z is an unfilled thermoplastic alloy with good weatherability and chemical resistance.Information provided by Celanese
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3035JX47 Plasticized Industrial Grade Nylon 12
Description: UBE UBESTA® Industrial grade Nylon 12Comments: conductiveInformation provided by UBE.
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Vandar® 2100UV PBT, Impact Modified  (Unverified Data**)
Vandar 2100UV is a polyester alloy designed to offer maximum impact strength at room and low temperatures. This unfilled compound is characterized by outstanding chemical resistance, dimensional sta..
Zone 1 230 - 240 °C
446 - 464 °F
Celanese Celanex® 6035GB20 PBT, 20% Glass Bead Filled
20% glass bead filled PBT.Information provided by Celanese Corporation.
Copyright © lookpolymers.com All Rights Reserved