Polymer Property : Zone 1 = 446 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 1 230 °C
446 °F
Die
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound
PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 1 230 - 260 °C
446 - 500 °F
hopper
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,..
Zone 1 230 - 250 °C
446 - 482 °F
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Saturate Sodium Chloride for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Toluene for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Water for 500 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® 3030U Nylon 12 (After Zinc chloride aq. for 1000 hours)
Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c..
Zone 1 230 - 240 °C
446 - 464 °F
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded
Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Zone 1 230 - 240 °C
446 - 464 °F
Eurostar Staramide PFB42U PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42U is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 1 230 °C
446 °F
For 8x1 mm Tube Extrusion
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12
Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System..