Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Melting Point 225 °C
437 °F
ASTM D3418
Celanese Celanex® 3300-2FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300-2FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outs..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celanex® 5300-2 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 5300-2 is a 30% fiberglass reinforced polyester with improved surface finish. Celanex 5300-2 contains an internal lubricant.30% glass reinforced, high gloss, general purpose, lubricatedInfor..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1,-2,-3
Celanese Celanex® 6500 PBT, 30% Mineral / Glass Reinforced  (Unverified Data**)
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability.30% glass/mineral, low warpInformation provided by Celanese
Melting Point 225 °C
437 °F
ASTM D3418
Celanese Vandar® 4662Z PBT, 30% Glass Reinforced  (Unverified Data**)
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Melting Point 225 °C
437 °F
@ Break; ASTM D3418
LG Chemical Lupox® GP2156FL PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by..
Melting Point 225 °C
437 °F
@ Break; ASTM D3418
LG Chemical Lupox® GP2400G PBT+GF40%
Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical
Melting Point 225 °C
437 °F
@ Break; ASTM D3418
LG Chemical Lupox® SG5200 PBT+PET+GF20%
Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Lanxess Pocan® KU 2-7604 000000 PBT+PC
PBT+PC, non-reinforced, injection molding, extrusion, flame retardant, impact modified, low tendency to warp
Melting Point 225 °C
437 °F
ASTM D3418
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT
Information provided by A. Schulman.
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
DSM Arnite® TV4 270 PBT-35% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Crastin® SK642FR BK851 Polybutylene Terephthalate (PBT)
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR BK851 is a black 15% glass fiber reinforced flame retardant polybutylene terephthalate for injection molding. It has a..
Melting Point 225 °C
437 °F
[10 K/min], ISO 11357
Eurotec® Tecodur® PB70 GR25 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Melting Point 225 - 250 °C
437 - 482 °F
10 K/min; ISO 3146
Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Barlog Plastics KEBATER A9045 PBT, 45% glass fiber reinforced, improved surface quality, reduced warpage, food grade
(PBT+X)-GF45Information provided by BARLOG plastics GmbH.
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Barlog Plastics KEBATER BM240 PBT, 40% mineral reinforced, food grade
(PBT+X)-MD40Information provided by BARLOG plastics GmbH.
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 1700A PBT, Unfilled
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Information provided by Celanese
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 3300D PBT, 30% Glass Reinforced
Celanex 3300D is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 3300FC PBT, 30% Glass Reinforced
Celanex 3300FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1,-2,-3
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 3400-2 PBT, 40% Glass Reinforced
Celanex 3400-2 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding..
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Melting Point 225 °C
437 °F
ASTM D3418
Celanese Celanex® 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.To avoid hydrolytic degradation during processing, ..
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 3316 PBT, 30% Glass Reinforced
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Melting Point 225 °C
437 °F
ISO 11357-1,-2,-3
Celanese Celanex® 2002UV PBT, Unfilled
Celanex 2002UV is a general purpose,unreinforced polybutylene terephthalate with a good balance of mechanical properties, processability and UV resistance. Celanex 2002UV is a medium flow materialTo..
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
DSM Arnite® TV4 260 S PBT-30% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX 4306 PBT, 30% Glass Reinforced
Celanex 4306 is a 30% glass reinforced, toughened, low warpage thermoplastic polyester.Information provided by Celanese
Melting Point 225 °C
437 °F
ASTM D3418
Celanese CELANEX J600 PBT, 40% Mineral / Glass Reinforced
Celanex J-600 is a 40% glass/mineral reinforced resin providing excellent warpage resistance, surface gloss and good mechanical properties. Celanex J-600 is particularly suited to applications requi..