Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 4.00 mm |
0.018 in/in @Thickness 0.157 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 2.00 mm |
0.018 in/in @Thickness 0.0787 in |
ISO 294-4 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 3.20 mm |
0.018 - 0.022 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | 60x60x2 mm; ISO 294-4 |
Gromax BTE90-DN001N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004 is a compound based on Nylon 66 resin containing PTFE. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.023 cm/cm | 0.018 - 0.023 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RL004S is a compound based on Nylon 66 resin containing PTFE. Added features of this material include: Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Elastoblend® POM CO IM MB Availability: North AmericaForms: PelletsAdditive: Impact Modifier Features: Impact Modified and CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® PA6/6 FR 346 RD Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 E4 A1 Nylon 66 Availability: North AmericaForms: PelletsFeatures: High ViscosityInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Luriblend® POM CO TL10 Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(10%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill FR® HDPE FR-2 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Thickness 3.17 mm |
0.018 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6/6 L N MB Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle and Nucleated TPCI# 8384101Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East) LNP *THERMOCOMP* PB006EQ is a compound based on PA 6 containing Glass Bead. Added features include Reduced Moisture. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2S 25 W 20 HL X black 9992 PA610 Product Description: Grilamid 2S 25 W 20 HL X black 9992 is a semi-flexible high viscosity heat stabilized, impact modified and plasticized Polyamide 610, especially suitable for extrusion applicati.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | Sim. To ISO 294-4 |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S600F10 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 BK851 is an unreinforced lubricated medium high viscosity black polybutylene tere.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.022 cm/cm @Thickness 4.00 mm |
0.018 - 0.022 in/in @Thickness 0.157 in |
E2P method |
Eurostar Star L PA D51 PA6, Injection Molded Star L PA6 D51 is a 15% PTFE Lubricated Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ASTM D955 |
Clariant Renol 6001 HV HSL Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm | 0.018 in/in | ISO 2577 |
BASF Ultradur® B 4520 High Speed PBT Description: Very easy flowing unreinforced injection molding grade with enhanced elongation for thin-walled parts (e.g. automotive connectors, switches, relay parts)Information provided by BASF |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Linear Mold Shrinkage, Flow | 0.018 cm/cm @Diameter 2.00 mm |
0.018 in/in @Diameter 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |