Polymer Property : Zone 2 = 235 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1600A PBT  (Unverified Data**)
Celanex 1600A is a high molecular weight grade of unreinforced polybutylene terephthalate used in both extrusion and injection molding applications.Extrusion gradeInformation provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2001FC PBT  (Unverified Data**)
Celanex 2001FC is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications for use in food contact applications...
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2016 PBT  (Unverified Data**)
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 2104UV PBT, UV Resistant  (Unverified Data**)
Celanex 2104UV is an unreiforced, impact modified, UV stabilized PBT designed for outdoor agricultural, industrial and automotive applications. Celanex 2104UV is suitable for injection molding appli..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3100-2 PBT, 7.5% Glass Reinforced  (Unverified Data**)
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.7.5% glass-f..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.15% glass-fiber, improved impactInformation provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4300 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300 is a toughened, 30% glass reinforced PBT.30% glass-fiber, good impact strengthInformation provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Vandar® 2500 PBT  (Unverified Data**)
Vandar 2500 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is specially designed to offer excellent chemical resistance, good colorability and dimensional ..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Vandar® 4662Z PBT, 30% Glass Reinforced  (Unverified Data**)
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Zone 2 235 °C
455 °F
Extrusion Coating
DuPont™ Elvaloy® AC 2618 Ethylene Methyl Acrylate
Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 1400FC PBT, Unfilled
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 1700A PBT, Unfilled
Celanex 1700A is a very high molecular weight grade of unreinforce polybutylene terephthalate for extrusion applications.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2001 PBT, Unfilled
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2002 PBT, Unfilled
Celanex 2002 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002 ia a medium flow material.Information provide..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3309HR PBT, 30% Glass Reinforced
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.Information provided by C..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3425HRT PBT, Glass Reinforced
Celanex 3425HRT is a non-lubricated, 40% fiberglass reinforced PBT copolymer that has excellent hydrolysis resistance, toughness, improved flow, and improved elongation at break.Information provided..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4202 PBT, 15% Glass Reinforced
Celanex 4202 is a 15% glass reinforced, impact modified polybutylene terephthalate with excellent surface appearance.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4306UV PBT, 30% Glass Reinforced
Celanex 4306UV is a 30% glass reinforced, toughened, low warpage, UV stable thermoplastic polyester.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese Cor..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3314 PBT, 30% Glass Reinforced
Celanex 3314 is a non-exuding (UL approved V-0 at 1/64 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is w..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3409HR PBT, 40% Glass Reinforced
Celanex 3409HR is a non-lubricated, 40% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degra..
Zone 2 235 - 255 °C
455 - 491 °F
Celanese Celanex® 6500LM PBT, 30% Mineral / Glass Reinforced
Celanex 6500 is a 30% glass/mineral polyester with improved surface finish and a good balance of mechanical properties and processability, that is also enhanced for improved laser marking graphics.T..
Zone 2 235 - 255 °C
455 - 491 °F
Celanese CELANEX 6407 PBT, 30% Mineral / Glass Reinforced
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.Information ..
Zone 2 235 - 255 °C
455 - 491 °F
Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced
Information provided by Celanese Corporation.
Zone 2 235 - 245 °C
455 - 473 °F
Eurostar Star L PA6 D83 PA6, Injection Molded
Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese Corporation.