Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
Plastcom PLASTAMID® 610 BT N 32 C PA610 Basic type PA610 for injection molding, modified for general use. Use: extrusion, filaments, injection molding. Delivered in the natural color.Information Provided by Plastcom spol. s r.o. |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH T20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TP-G40 Polybutylene Terephthalate, 40% Glass Reinforced Polybutylene Terephthalate, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Melt Temperature | 170 - 260 °C | 338 - 500 °F | |
NOVA Chemicals Sclair® 2815 HDPE Injection Molding Resin Features: Excellent balance of stiffness and toughness, low odor.Applications: Margarine and spreads, thin walled containers, frozen food containers.Data provided by the manufacturer. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4700 AR 15 TFE 15 Polytrimethylene Terephthalate (PTT), Aramid Fiber - PTFE Lubricated |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH GF5040 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Temperature | 205 - 260 °C | 401 - 500 °F | |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | Stock |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU.. |
|||
Melt Temperature | 254 - 260 °C | 489 - 500 °F | Tubular (Blown) Film |
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well .. |
|||
Melt Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Melt Temperature | 235 - 260 °C | 455 - 500 °F | Start Point: 250°C |
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |
|||
Melt Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 250°C |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 246 - 260 °C | 475 - 500 °F | |
LyondellBasell Petrothene® LR590005 High Density Polyethylene ApplicationsPETROTHENE LR 5900-05 is a high density, high molecular weight resin designed for primary insulation for electronic cables. This resin exhibits low shrinkback after extrusion, contains .. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | ISO 294 |
Styrolution Terluran® HI-12 ABS Terluran HI-12 is an injection molding grade of ABS with a very high toughness and easy flow.Very high toughnessEasy flowingUL 94 HB (1.6 & 3.2 mm)Information provided by Styrolution |
|||
Melt Temperature | 210 - 260 °C | 410 - 500 °F | |
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled Daplen KSR65T20 is a 20% mineral filled grade for injection molding. Daplen KSR65T20 has been developed especially for the car industry, to be used in interior parts. Daplen KSR65T20 offers very g.. |
|||
Melt Temperature | 220 - 260 °C | 428 - 500 °F | |
TPI Porene® KU900 Super High Heat ABS INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymer.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | Extrusion |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 2099 X 115387 A Biobased Polyamide (PA) Glass Fiber - 43% Bio-Content |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Ecomass® 1850ZN66T1 Steel Powder Filled Polyamide, Injection Molding Steel Powder Filled Polyamide (PA6), Impact Modified, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInformation provide.. |
|||
Melt Temperature | 245 - 260 °C | 473 - 500 °F | |
CP-Polymer-Technik Wellamid® 6000/50 CP Nylon 6, Impact Modified Until 0°C, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Melt Temperature | 235 - 260 °C | 455 - 500 °F | |
Celanese CELANEX 3400 PBT, 40% Glass Reinforced Celanex 3400 is a general purpose, 40% glass reinforced polybutylene terephthalate that offers a good combination of mechanical, electrical, and thermal properties. This grade provides outstanding p.. |
|||
Melt Temperature | 235 - 260 °C | 455 - 500 °F | |
Celanese CELANEX 2104UV PBT, UV Resistant Celanex 2104UV is an unreiforced, impact modified, UV stabilized PBT designed for outdoor agricultural, industrial and automotive applications. Celanex 2104UV is suitable for injection molding appli.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company RTP 4799 X 117571 E Polytrimethylene Terephthalate (PTT) Glass Fiber - Flame Retardant - Halogen Free |
|||
Melt Temperature | 235 - 260 °C | 455 - 500 °F | Injection Molding |
DuPont Performance Polymers Crastin® S610SF NC010 PBT
(Unverified Data**) Crastin® S610SF is an unreinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast production.Informati.. |
|||
Melt Temperature | 232 - 260 °C | 450 - 500 °F | |
RTP Company VLF 84709 Polytrimethylene Terephthalate (PTT), Long Glass Fiber
(discontinued **) Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |