Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66 Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app.. |
|||
Drying Temperature | 79.4 - 85.0 °C | 175 - 185 °F | |
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Drying Temperature | 79.4 - 85.0 °C | 175 - 185 °F | |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-G50 Nylon 66, 50% Glass Reinforced Nylon 66, 50% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Average value: 80.0 °C Grade Count:4 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |
|||
Drying Temperature | 80.0 - 85.0 °C @Time 7200 - 10800 sec |
176 - 185 °F @Time 2.00 - 3.00 hour |
|
IRPC Polimaxx Polene 129PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP, ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Drying Temperature | 82.2 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Drying Temperature | 82.0 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS 3003 MC Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide P1000EI3 PA6, Impact Modified, Injection Molded Staramide P1000EI3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020)Information provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Starflam RF0069 PA66, 30% Glass Fiber, Flame Retardant, Injection Molded Starflam RF0069 is a Flame Retardant, 30% Glass Reinforced Polyamide 66 Injection Molding Resin (also known as PA66 30V U2 Z79 or RF1006Z590)Information provided by Eurostar. |
|||
Drying Temperature | 79.4 - 85.0 °C | 175 - 185 °F | |
Engineered Polymer Solutions ABS PCR 400, Recycled General Purpose with 40% Post Consumer ABS. Natural and colors available. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
Drying Temperature | 71.1 - 85.0 °C | 160 - 185 °F | or lower with overnight predrying |
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas.. |