Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid B3 H ZC Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66 Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Drying Temperature | 73.9 - 85.0 °C | 165 - 185 °F | |
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
PolyOne Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Drying Temperature | 80.0 - 85.0 °C @Time 7200 - 14400 sec |
176 - 185 °F @Time 2.00 - 4.00 hour |
Pre-dry |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GN1000FA PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 181028-79-5Information provided by .. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | Injection Molding |
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Drying Temperature | 82.2 - 85.0 °C | 180 - 185 °F | |
Styron MAGNUMâ„¢ 342 EZ Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 342 EZ ABS resin is a medium impact, high flow, low gloss resin often used in automotive applications. Automotive MAGNUM ABS resins offer a wide range of gloss, viscosity, imp.. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS 1002 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl.. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Drying Temperature | 75.0 - 85.0 °C | 167 - 185 °F | |
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Starflam A28UL PA66, Flame Retardant, Injection Molding Staramide A28UL is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Starflam P10002Z PA6, Flame Retardant, Extrusion Starflam P10002Z is an Unfilled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Extrusion ResinInformation provided by Eurostar. |
|||
Drying Temperature | 80.0 - 85.0 °C | 176 - 185 °F | |
Diamond Polymers ASA TWP 502 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Drying Temperature | 70.0 - 85.0 °C | 158 - 185 °F | Average value: 75.0 °C Grade Count:6 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Drying Temperature | 75.0 - 85.0 °C @Time 14400 - 21600 sec |
167 - 185 °F @Time 4.00 - 6.00 hour |
|
Eurostar Staramide BG3ST42 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG3ST42 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |