Processing Properties Metric English Comments
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3300-2LM PBT, Glass Reinforced  (Unverified Data**)
Celanex 3300-2LM is a 30% glass-filled PBT that is enhanced for improved laser marking graphics. It contains an internal lubricant for enhanced mold release.30% glass-filled PBT, laser markableInfo..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3309HR PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass reinforced, hyd..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3309HRLM PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HRLM is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass filled PBT, h..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4300 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300 is a toughened, 30% glass reinforced PBT.30% glass-fiber, good impact strengthInformation provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 4309AR PBT  (Unverified Data**)
Information provided by Celanese
Zone 2 235 - 255 °C
455 - 491 °F
Celanese Celanex® 5200-2 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.15% glass reinforced, high gloss, general purpose, lubricatedInfor..
Zone 2 235 - 255 °C
455 - 491 °F
Celanese Celanex® 5202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 531HS PBT, Glass Reinforced  (Unverified Data**)
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Zone 2 235 °C
455 °F
Extrusion Coating
DuPont™ Elvaloy® AC 2618 Ethylene Methyl Acrylate
Elvaloy® AC 2618 is a copolymer of ethylene and ethyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® AC..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 1700FC PBT, Unfilled
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2002-2 PBT, Unfilled
Celanex 2002-2 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 2002-2 ia a medium flow material that contains a..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 2008 PBT, Unfilled
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by ..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3100-2 PBT, 7.5% Glass Reinforced
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.Information ..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3300FC PBT, 30% Glass Reinforced
Celanex 3300FC is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityInformation provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3309HR PBT, 30% Glass Reinforced
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.Information provided by C..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4306UV PBT, 30% Glass Reinforced
Celanex 4306UV is a 30% glass reinforced, toughened, low warpage, UV stable thermoplastic polyester.Information provided by Celanese
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3201 PBT, 15% Glass Reinforced
Celanex 3201 is a 15% glass reinforced general purpose thermoplastic polyester resin that offers a superior combination of mechanical, electrical, and thermal properties, together with outstanding p..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese VANDAR 2500 PBT, Unfilled
Vandar 2500 is an unfilled polyester alloy which exhibits excellent toughness and impact strength. It is specially designed to offer excellent chemical resistance, good colorability and dimensional ..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 4016 PBT, Unfilled
Non-exuding, unfilled, flame retardant polybutylene terephthalate which has an excellent balance of mechanical properties and processability. Celanex 4016 is well suited for applications requiring i..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese CELANEX 6035GB20 PBT, 20% Specialty
20% glass bead filled PBT.Information provided by Celanese
Zone 2 235 - 255 °C
455 - 491 °F
Celanese CELANEX 6400-2 PBT, Mineral / Glass Reinforced
40% glass/mineral reinforced polyester, providing warp resistance and improved surface finish.Information provided by Celanese
Zone 2 235 - 255 °C
455 - 491 °F
Celanese CELANEX 6407 PBT, 30% Mineral / Glass Reinforced
Celanex 6407 is a 30% glass/mineral reinforced resin perticularly suited for large exterior automotive components, where extended flow, flatness and good surface appearance is essential.Information ..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 3309HRHF PBT, 30% Glass Reinforced
Celanex 3309HRHF is a 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and improved flow.Information provided by Celanese Corpora..
Zone 2 235 - 255 °C
455 - 491 °F
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Zone 2 235 - 250 °C
455 - 482 °F
Celanese Celanex® 1600FC PBT  (Unverified Data**)
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Zone 2 235 - 255 °C
455 - 491 °F
Celanese Celanex® J600 PBT, 40% Mineral / Glass Reinforced  (Unverified Data**)
Celanex J-600 is a 40% glass/mineral reinforced resin providing excellent warpage resistance, surface gloss and good mechanical properties. Celanex J-600 is particularly suited to applications requi..