Polymer Property : Linear Mold Shrinkage, Flow = 0.018 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Horizontal
PTS POM-25 Acetal Copolymer
Information provided by PTS LLC.
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® S650FR BK851 PBT  (Unverified Data**)
Crastin® S650FR is an unreinforced, black, flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® ST820 BK503 PBT  (Unverified Data**)
Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.20 mm
0.018 in/in

@Thickness 0.126 in
ASTM D955
LG Chemical Lupox® GP1000A PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer
LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant.
Linear Mold Shrinkage, Flow 0.018 - 0.023 cm/cm
0.018 - 0.023 in/in
on Tensile Bar; SABIC Method
SABIC Innovative Plastics LNP LUBRICOMP RFL46 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFL46 is a compound based on PA66 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Luriblend® PA6/6 TS18 Nylon 66
Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Luriblend® POM CO TL15 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and CopolymerInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Plastiblend® PA6/6 HS L N Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and Nucleating AgentFeatures: Heat Stabilized, Impact Modified and NucleatedProcessing Method: Injection MoldingIn..
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Statiblend® POM CO
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Crastin® S600F10 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 BK851 is an unreinforced lubricated medium high viscosity black polybutylene tere..
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)  (Unverified Data**)
Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio..
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® ST800HSL BK152 Nylon 66  (Unverified Data**)
Super Toughened Heat Stabilized Polyamide 66 Zytel ST800HSL BK152 is a heat stabilized Super Tough black polyamide 66 resin. It offers outstanding impact resistance high productivity and laser marka..
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
ASTM D955
Clariant Renol PA2SP0004 Nylon 6 Alloy
Data provided by Clariant Masterbatches
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
ISO 2577
BASF Ultraform® N2640 E4 POM
Description: Is a POM + MBS, elastomer-modified injection-molding grade with high toughness and high weld line strength.Information provided by BASF
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, Conditioned
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
Horizontal
BLUESTAR BS270 Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Diameter 2.00 mm
0.018 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Linear Mold Shrinkage, Flow 0.018 - 0.022 cm/cm

@Thickness 4.00 mm
0.018 - 0.022 in/in

@Thickness 0.157 in
E2P method
Eurostar Star L PA6 D83 PA6, Injection Molded
Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.