DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/Nylon 6 Blend, Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Zytel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was developed for applications requiring strength stiffness and iInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
DAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
DAM; ISO 294-4 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell M 53
53
50%RH; ISO 2039-2
81
81
DAM; ISO 2039-2
Hardness, Rockwell R 113
113
50%RH; ISO 2039-2
116
116
DAM; ISO 2039-2
Tensile Strength at Break 115 MPa
16700 psi
50%RH; ISO 527-1/-2
150 MPa
21800 psi
DAM; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
DAM; ISO 527-1/-2
8.6 %
8.6 %
50%RH; ISO 527-1/-2
Tensile Modulus 6.929 GPa
1005 ksi
50%RH; ISO 527-1/-2
9.00 GPa
1310 ksi
DAM; ISO 527-1/-2
Flexural Modulus 5.60 GPa
812 ksi
50%RH; ISO 178
7.68 GPa
1110 ksi
DAM; ISO 178
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
DAM; ISO 180/1A
23.0 kJ/m²
10.9 ft-lb/in²
50%RH; ISO 180/1A
12.0 kJ/m²

@Temperature -40.0 °C
5.71 ft-lb/in²

@Temperature -40.0 °F
50%RH; ISO 180/1A
15.0 kJ/m²

@Temperature -40.0 °C
7.14 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
50%RH; ISO 179/1eA
2.10 J/cm²
9.99 ft-lb/in²
DAM; ISO 179/1eA
1.00 J/cm²

@Temperature -40.0 °C
4.76 ft-lb/in²

@Temperature -40.0 °F
50%RH; ISO 179/1eA
1.10 J/cm²

@Temperature -40.0 °C
5.23 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C
66.7 µin/in-°F
DAM; ISO 11359-1/-2
Melting Point 250 °C
482 °F
DAM; 10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 247 °C
477 °F
DAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 222 °C
432 °F
DAM; ISO 75-1/-2
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
DAM; IEC 60695-11-10
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
DAM; IEC 60695-11-10
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
DAM; IEC 60112
Descriptive Properties Value Comments
Delivery Form Pellets
Part Marking Code >PA66+PA6-IGF33<
ISO 11469
Processing Injection Moulding
Regional Availability North America
South and Central America
Resin Identification PA66+PA6-IGF33