NOVA Chemicals Novapol® HB-L455-A HDPE Blow Molding Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HB-L455-A HDPE Blow Molding Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Plaque Properties. Features: excellent processability on high speed, multiple-head blow molding lines, good balance of physical and molding properties.Applications: chemical bottles, toys.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D792
Environmental Stress Crack Resistance 25 hour
25 hour
F50, Condition A, ASTM D1693, 100% Igepal
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 800 %
800 %
ASTM D638
Flexural Modulus 1.22 GPa
177 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm
3.93 ft-lb/in
Notched/Unnotched not specified; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 160 - 205 °C
320 - 401 °F