Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® HMG47MD ABS General purpose, injection molding ABS for medical applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ADX1016R PC (Europe-Africa-Middle East) Lexan Copolymer resin with improved chemical resistance, available only in limited colors. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP HF006EU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF006EU is a compound based on PA 11 resin containing Glass Fiber. Added features include: Easy Molding, UV-Stabilized. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PCAF04FRHH PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* PCA04FRHH is a 20 % glass reinforced PC+ABS blend without chlorinated or brominated flame retardants. LNP* THERMOCOMP* complies with the material requirements as specified in TCO'99.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -40.0 °C |
10.9 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS (Asia Pacific) LNP* Verton* NV003E is a compound based on PC+ABS Blend resin containing Long Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RVL28 PA 66 LNP* VERTON* RVL28 is a compound based on Nylon 66 resin containing 40% Long Glass Fiber, 10% PTFE. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant, Structura.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | Low Temp; ISO 180/1eA |
Lubrizol ESTALOC® 59600 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -50.0 °C |
10.9 ft-lb/in² @Temperature -58.0 °F |
|
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature 23.0 °C |
10.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Izod Impact, Notched (ISO) | 23.0 - 97.0 kJ/m² @Temperature -50.0 - -50.0 °C |
10.9 - 46.2 ft-lb/in² @Temperature -58.0 - -58.0 °F |
Average value: 44.5 kJ/m² Grade Count:8 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON RVN17SXS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RVN17SXS is a compound based on PA 66 resin containing Long Glass Fiber, MoS2. Added features include; Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-746Y ABS
(discontinued **) Medium flow, high impact |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East) PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² @Temperature -30.0 °C |
10.9 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND PCA 628 PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Extrusion grade with very good toughness. Main application fields: automotive small profilesUnfilled. Suitable for Extrusion, Thermoforming. Supplied as pe.. |
|||
Izod Impact, Notched (ISO) | 23.0 kJ/m² | 10.9 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |