Polymer Property : Izod Impact, Notched (ISO) = 9.99 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific)
Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex..
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature -30.0 °C
9.99 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific)
Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, Conditioned
Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer (Europe-Africa-Middle East)
LNP* LUBRICOMP* YL003 is a compound based on Polyester Elastomer containing PTFE. Added features include; Internally Lubricated.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON DX11408 PC
LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific)
LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS (Asia Pacific)
LNP* Verton* NV003E is a compound based on PC+ABS Blend resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA
High flow PPO+PA. Power distribution box applications.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific)
High flow PPO+PA. Power distribution box applications.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11
LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON MV00ASXC PP (Europe-Africa-Middle East)
LNP* VERTON* MV00ASXC is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON NV003E PC+ABS
LNP* VERTON* NV003E is a compound based on PC+ABS Blend resin containing 15% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East)
Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating ..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
Conditioned; ISO 180/1A
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6
Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay.
Izod Impact, Notched (ISO) 21.0 kJ/m²

@Temperature 23.0 °C
9.99 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
DSM Arnitel® PL650 Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1A
Chi Mei Polylac® PA-717C ABS
Medium impact
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L BK104 is a 33% glass fiber reinforced heat stabilized black polyamide 66 resin with outstanding impact resistance develope..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6  (Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO 180/1A
Chi Mei Polylac® PA-727 ABS
Electro-plating
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
ISO Test
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RX00078 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX00078 is a compound based on PA 66 resin containing Long Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Izod Impact, Notched (ISO) 21.0 kJ/m²
9.99 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics GELOY XP4025 ASA+PC
Available in a wide range of colors and is recommended for unpainted exterior applications.