Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYblend 65FS GF20 PC/ABS-Blend Information provided by Polykemi AB |
|||
Flexural Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF1030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A13^ FX30 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL34XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL-4034 HP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Flexural Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 5.60 GPa @Temperature 23.0 °C |
812 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF4030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
Nilit FRIANYL A63 H-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178-A |
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2mm/min; ASTM D790 |
Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesExcellent size stabilityNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInforma.. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP HF006EU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF006EU is a compound based on PA 11 resin containing Glass Fiber. Added features include: Easy Molding, UV-Stabilized. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6 LNP THERMOCOMP* PF003 is a compound based on Nylon 6 resin containing 15% Glass Fiber. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® SHF4340 PBT 20% GF Super High Flow PBT |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY WF306C PBT LNP* STAT-LOY* WF306C is a compound based on PBT resin containing 30% Glass Fiber. Added features of this material include: Antistat, Clean Compound System. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
Polyram RamTough PZ324G4NT Polycarbonate, 20% Glass Fiber, Flame Retardant 20% glass fiber reinforced, flame retardant polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced 30% Glass fiber reinforced Nylon6/PP alloy with reduced water absorption, dimensional stability and UV stabilized, for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 5.60 GPa @Temperature 180 °C |
812 ksi @Temperature 356 °F |
ISO 178 |
DSM Stanyl® OCD2300 BLK PA46-GF50 50% Glass Reinforced, Heat Stabilized |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop.. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 109 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |