Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Asia Pacific) Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature 0.000 °C |
7.14 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® RCY6713 PC (Asia Pacific) Cycoloy* RCY6713 resin is an injection moldable high heat PC blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.5.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP6REU PC (Europe-Africa-Middle East) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East) Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HPS7R PC (Europe-Africa-Middle East) Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Aardvark Polymers AARTEL® 1000 Rotational Molding Resin Aartel 1000 is our premium grade of toughened impact modified acetal copolymer. Aartel 1000 is formulated with high impact properties combined with extended mechanical properties and elevated resist.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | d.a.m.; ISO 180-1A |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | >= 15.0 kJ/m² | >= 7.14 ft-lb/in² | ISO 180-1A |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature 0.000 °C |
7.14 ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP TH0300B PU LNP* Thermocomp* Th0300B is a compound based on Polyurethane containing proprietary fillers. Characteristics of this grade are High Specific Gravity. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics XYLEX HX7409HP PC+POLYESTER Low flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change (MoC), biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 BK356 is a Super Tough heat stabilized lubricated black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO180/A |
BASF Ultramid® B3L PA6 (Dry) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl PMD 20143 Nylon 6 High impact resistanceInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ASTM D256 |
BLUESTAR LXS 314 G40 PPE-HIPS, 40% Glass Filled Typical Applications: Military industrial productsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Conditioned) Ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL FN150 PPE+HIPS (Europe-Africa-Middle East) NORYL FN150 twin wall foam meets UL standard 94 V-0/5V ratings at 4 mm wall thickness. These unique flammability characteristics make FN150 the supreme choice for designing optimum wall thickness in.. |
|||
Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF OF008I PPS - Linear (Europe-Africa-Middle East) LNP* Thermotuf* OF008I is a compound based on PPS - Linear resin containing Glass Fiber. Added features of this material include: High Impact. |