ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Elastomer, TPE , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name EXXELOR™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXXELOR™ PO 1015 Maleic anhydride functionalized polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exxelor Po 1015 polymer resin is a maleic anhydride fuctionalized polypropylene copolymer, produced by reactive extrusion. It has been primarily designed to add polarity to polypropylene matrices and in particular improved polypropylene reactivity and amio-silane treated glass reinforcements. This grade is designed to:Function as a coupling agent between reinforcing materials such as glass fibers and inorganic fillers, and polypropylene.Achieve compatibility in polypropylene/polyamide alloys. Achieve compatibility between polyolefins and more polar polymers that are capable of interaction with maleic anhydride for alloying recycling or co-extrusion purpose.Improve polypropylene-to-metal adhesion properties.Key Features: Performance enhancements in glass-filled polypropylene:Outstanding unnotched Izod and Charpy impact performanceExcellent notched Izod and Charpy impact resistanceImproved tensile and flexural strengthAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
DIN 53479
Melt Flow 22 g/10 min

@Load 1.20 kg,
Temperature 190 °C
22 g/10 min

@Load 2.65 lb,
Temperature 374 °F
ASTM D1238
150 g/10 min

@Load 2.16 kg,
Temperature 190 °C
150 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Collected Volatile Condensable Material <= 0.20 %
<= 0.20 %
AM-S 350.03
Thermal Properties Metric English Comments
Melting Point 138 °C
280 °F
Peak; DSC
Optical Properties Metric English Comments
Yellow Index <= 20 %
<= 20 %
ASTM E313-96
Descriptive Properties Value Comments
Maleic anhydride graft level medium