Material Notes:
Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or steam at high temperature. Catalyst CT 0552/09 contains a processing aid.Features: Antioxidant; Good Thermal Aging ResistanceUses: Connectors; Hose; Potable Water ApplicationsAdditional Properties: Extruder Screw Compression Ratio - >2.5:1; Extruder Screw L/D Ratio - 25:1 to 30:1; Head Temperature - 200 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Apparent Bulk Density 0.550 g/cc
0.0199 lb/in³
ASTM D1895
Melt Flow 1.5 g/10 min
1.5 g/10 min
ISO 1133
Processing Properties Metric English Comments
Zone 1 150 - 200 °C
302 - 392 °F
Zone 2 150 - 200 °C
302 - 392 °F
Zone 3 150 - 200 °C
302 - 392 °F
Zone 4 150 - 200 °C
302 - 392 °F
Zone 5 150 - 200 °C
302 - 392 °F
Die Cooling Temperature 210 °C
410 °F
Descriptive Properties Value Comments
Agency Ratings DVGW W270; KTW Unspecified Rating
Availability Asia Pacific
Europe
North America
Processing Technique Extrusion; Pipe Extrusion