DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer

Category Polymer , Film , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Molding Grade
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Elvaloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing properties and has high filler acceptance.Elvaloy® 1218 AC is easily processed on standard equipment used for low-density polyethylene.Information provided by DuPont.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792 - ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
ASTM D2240 - ISO 868
Hardness, Shore D 35
35
ASTM D2240 - ISO 868
Tensile Strength at Break 13.0 MPa
1890 psi
500 mm/min; ASTM D638 - ISO 527-2
Elongation at Break 600 %
600 %
500 mm/min; ASTM D638 - ISO 527-2
Tensile Modulus 0.0450 GPa
6.53 ksi
1 mm/min; ASTM D638 - ISO 527-2
Thermal Properties Metric English Comments
Melting Point 94.0 °C
201 °F
By DSC; ASTM D3418 - ISO 3146
Vicat Softening Point 60.0 °C
140 °F
A<sub>50</sub> (10N); ASTM D1525 - ISO 306
Processing Properties Metric English Comments
Rear Barrel Temperature 150 °C
302 °F
Extrusion lamination and extrusion coating
150 °C
302 °F
Cast film
150 °C
302 °F
Blown film
Middle Barrel Temperature 160 °C
320 °F
Blown film
210 °C
410 °F
Cast film
220 °C
428 °F
Extrusion lamination
Front Barrel Temperature 170 °C
338 °F
Blown film
250 °C
482 °F
Cast film
290 °C
554 °F
Extrusion lamination
Adapter Temperature 180 °C
356 °F
Blown film
250 °C
482 °F
Cast Film
290 °C
554 °F
Extrusion lamination
Die Temperature 180 °C
356 °F
Blown film
250 °C
482 °F
Cast film
290 °C
554 °F
Extrusion lamination
Descriptive Properties Value Comments
MA-Content 18 wt.%
DuPont Method