Polymer Property : Die Temperature = 356 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 180 - 200 °C
356 - 392 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Die Temperature 180 - 205 °C
356 - 401 °F
Extrusion
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Die Temperature 180 - 195 °C
356 - 383 °F
Extrusion Molding
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionInjection: Cable sheathing, Highly Pressurized HoseIndustry Parts Information provided by API-Kolon.
Die Temperature 180 °C
356 °F
Taiwan PU Corporation TPU-CH75 High Hydrolysis Resistance, Calender Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Die Temperature 180 - 200 °C
356 - 392 °F
Extrusion
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Die Temperature 180 - 200 °C
356 - 392 °F
Extrusion
Stellarchem GP-950 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Die Temperature 180 - 200 °C
356 - 392 °F
Extrusion
Stellarchem MP-845B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Die Temperature 180 - 200 °C
356 - 392 °F
Extrusion
Stellarchem MP-855WR TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Die Temperature 180 - 220 °C
356 - 428 °F
Borealis BB125MO Polypropylene Copolymer
BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a..
Die Temperature 180 - 220 °C
356 - 428 °F
Borealis BL2571 High Density Polyethylene
BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers..
Die Temperature 180 °C
356 °F
6, Zone 1, Extrusion
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables..
Die Temperature 180 °C
356 °F
Borealis LE0563 Polyethylene Compound, Thermoplastic, Semiconductive
LE0563 is a thermoplastic semi conductive compound specifically designed for medium- and high voltage cable systems requiring improved grounding. It may be used either as a complete jacket or as a t..
Die Temperature 180 - 220 °C
356 - 428 °F
Borealis RB307MO Polypropylene Random Copolymer
RB307MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. This grade also features high heat distortion temperature. Applications: household and..
Die Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..
Die Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent ..
Die Temperature 180 - 220 °C
356 - 428 °F
Borealis BS4641 High Density Polyethylene
BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App..
Die Temperature 180 - 220 °C
356 - 428 °F
Borealis RB607MO Polypropylene Random Copolymer
RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion ..
Die Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer
Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The..
Die Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer
Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce..
Die Temperature 180 - 200 °C
356 - 392 °F
Elastron® G SEBS Elastomer
Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v..
Die Temperature 180 - 220 °C
356 - 428 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1556A Copolyamide Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 180 - 220 °C
356 - 428 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1564A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications)
GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r..
Die Temperature 180 - 230 °C
356 - 446 °F
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline ..
Die Temperature 180 - 220 °C
356 - 428 °F
Borealis RB206MO-06 Polypropylene Random Copolymer
RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als..
Die Temperature 180 °C
356 °F
6, Extrusion
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant
Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Transparent spherical pelletsFeatures: Zero halogenUses..