Polymer Property : Front Barrel Temperature = 482 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 250 °C
482 °F
NYCOA 1637 PA 6
plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc.
Front Barrel Temperature 250 °C
482 °F
NYCOA 1838 Copolymer Nylon Alloy
good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc.
Front Barrel Temperature 250 °C
482 °F
NYCOA 2012 Copolymer Nylon
easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc.
Front Barrel Temperature 250 °C
482 °F
NYCOA 2046 Copolymer Nylon 6/69
extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc.
Front Barrel Temperature 250 °C
482 °F
NYCOA 2237 Copolymer Nylon 6/66 Alloy
transparent molding and extrusion gradeInformation provided by NYCOA, Inc.
Front Barrel Temperature 250 °C
482 °F
NYCOA 400 PA 6
nucleated general molding gradeInformation provided by NYCOA, Inc.
Front Barrel Temperature 250 °C
482 °F
NYCOA 512 PA 6
UL and NSF rated nucleated general purpose molding gradeInformation provided by NYCOA, Inc.
Front Barrel Temperature 250 - 265 °C
482 - 509 °F
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Start Point: 255°C
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect..
Front Barrel Temperature 250 - 285 °C
482 - 545 °F
Start Point: 270°C
Kingfa JH720 G10 10% Glass Fiber Reinforced PC
Features:High mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanner cabinetComputer plug partsCD-ROM, DVDElectri..
Front Barrel Temperature 250 - 290 °C
482 - 554 °F
Start Point: 275°C
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC
Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne..
Front Barrel Temperature 250 - 270 °C
482 - 518 °F
Start Point: 260°C
Kingfa LONOY 6100 Flame Retardant PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to..
Front Barrel Temperature 250 - 260 °C
482 - 500 °F
Injection Molding
LG Chemical Lupox® SV1120M PBT
Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical
Front Barrel Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP5100 PC/ABS+GF10%
Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by..
Front Barrel Temperature 250 - 270 °C
482 - 518 °F
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy
Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Start Point: 255°C
Kingfa JH710 G20 Flame Retardant & 20% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Front Barrel Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP1000LG PC, Transparent
Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical
Front Barrel Temperature 250 - 265 °C
482 - 509 °F
Injection Molding
LG Chemical LUPOY GP1000M PC, Transparent
Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate
Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G..
Front Barrel Temperature 250 - 270 °C
482 - 518 °F
Unitika LM-8503-10
Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd.
Front Barrel Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 1125 AC Ethylene and 25% Methyl Acrylate Copolymer
Elvaloy® 1125 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..
Front Barrel Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Front Barrel Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go..
Front Barrel Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Front Barrel Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer
Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce..
Front Barrel Temperature 250 - 270 °C
482 - 518 °F
Unitika UM-8400-20
Characteristics: High dimensional accuracy (circularity and planarity) Large warping resistance Low linear expansion coefficientInformation provided by Unitika Ltd.
Front Barrel Temperature 250 - 270 °C
482 - 518 °F
Zone 3
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded
PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol..
Front Barrel Temperature 250 - 270 °C
482 - 518 °F
Zone 3
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded
PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo..
Front Barrel Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..
Front Barrel Temperature 250 °C
482 °F
For high temperature coextrusions.
DuPont Bynel® 50E631 Adhesive Resin  (discontinued **)
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru..