Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 4; Cylinder |
Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
Gichem GILAC C120/T Acrylonitrile Butadiene Styrene
(discontinued **) ABS with excellent thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Gichem GIBLEND F70500 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, excellent mechanical and thermal properties, very high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion Coating |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Middle Barrel Temperature | 220 - 230 °C | 428 - 446 °F | Start Point: 225°C |
Kingfa JE2-R2 ABS/PBT Alloy Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 225°C |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 235°C |
Kingfa MAC-851 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical XR474F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | H2 |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
DuPont Bynel® 3126 Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 6 30% Mineral Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Diamond Polymers ABS 3001MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Diamond Polymers ABS 3003 MC Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |