Mechanical Properties Metric English Comments
Tensile Modulus 0.0450 GPa

@Temperature 23.0 °C
6.53 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 4069 TPC-ET  (Unverified Data**)
Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection..
Tensile Modulus 0.0450 GPa
6.53 ksi
ISO 527
Lubrizol ESTANE® GP92AT Ether Based Thermoplastic Polyurethane
Type: Estane® GP 92AT is an aromatic polyether-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tensile Modulus 0.0450 GPa
6.53 ksi
1 mm/min; ASTM D638 - ISO 527-2
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Tensile Modulus 0.0450 GPa
6.53 ksi
ISO 527-1/-2
DSM Arnitel® XG6029 TPC-ET
Extrusion Grade
Tensile Modulus 0.0450 GPa
6.53 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Modulus 0.0450 GPa
6.53 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients..
Tensile Modulus 0.0450 GPa
6.53 ksi
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F5 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced Medium Viscosity Polyester Elastomer Information provided by DuPont Performance Polymers
Tensile Modulus >= 0.0450 GPa
>= 6.53 ksi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Tensile Modulus 0.0450 GPa
6.53 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver..
Tensile Modulus 0.0450 GPa
6.53 ksi
BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer
Product with properties which are typical of flexible PVC and of low density polyethylene. Suitable for flexible pipes, profiles and seals.Data was collected by ISO methods and provided by BASF.
Tensile Modulus 0.0450 GPa
6.53 ksi
1 mm/min
Arkema Group Evatane® 1350 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for molding very flexible articles. Examples: gaskets.ISO data provided by the manufacturer, Arkema.
Tensile Modulus 0.0450 GPa
6.53 ksi
average; in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.55 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Tensile Modulus 0.0450 GPa

@Temperature 23.0 °C
6.53 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® 4068FG TPC-ET  (Unverified Data**)