Material Notes:
3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for label material that offers excellent chemical resistance and holding strength even at high temperatures.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Adhesive
58.4 microns
2.30 mil
Facestock
94.0 microns
3.70 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.1205 kN/m
0.6875 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.1205 kN/m
0.6875 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.131 kN/m
0.750 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1424 kN/m
0.8125 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.20817 kN/m
1.1875 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.2410 kN/m
1.375 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.2410 kN/m
1.375 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.2410 kN/m
1.375 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.27391 kN/m
1.5625 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.27391 kN/m
1.5625 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.27391 kN/m
1.5625 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.2849 kN/m
1.625 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.33964 kN/m
1.9375 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.36156 kN/m
2.0625 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3725 kN/m
2.125 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.3725 kN/m
2.125 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.38347 kN/m
2.1875 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.38347 kN/m
2.1875 pli
Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.394 kN/m
2.25 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.394 kN/m
2.25 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.40538 kN/m
2.3125 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.42729 kN/m
2.4375 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.42729 kN/m
2.4375 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.438 kN/m
2.50 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5040 kN/m
2.875 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5478 kN/m
3.125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5478 kN/m
3.125 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.570 kN/m
3.25 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.58068 kN/m
3.3125 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.5916 kN/m
3.375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.66833 kN/m
3.8125 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.701 kN/m
4.00 pli
Smooth Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.71216 kN/m
4.0625 pli
Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.7231 kN/m
4.125 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.745 kN/m
4.25 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.75598 kN/m
4.3125 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.7669 kN/m
4.375 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.77789 kN/m
4.4375 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.789 kN/m
4.50 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.79981 kN/m
4.5625 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.8108 kN/m
4.625 pli
Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.82172 kN/m
4.6875 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.82172 kN/m
4.6875 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.88746 kN/m
5.0625 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.88746 kN/m
5.0625 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.90937 kN/m
5.1875 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.90937 kN/m
5.1875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.920 kN/m
5.25 pli
Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.964 kN/m
5.50 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
1.01 kN/m
5.75 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type #350 Acrylic
Liner 55# Clay coated kraft