Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 180 - 190 °C | 356 - 374 °F | Extrusion |
ExxonMobil Dytron™ XK7300-92 Thermoplastic Elastomer
(discontinued **) A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is flexible and halogen-free, and is intended mainly for extrusion of ca.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Die Temperature | 180 - 210 °C | 356 - 410 °F | |
Celanese Hostaform® MR130HPB POM, Specialty
(Unverified Data**) Preliminary Data SheetMedia resistant - bleach, high modulus gradeInformation provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9364 POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9364 is highly impact modified grade for demanding applications. Hostaform® S 9364 provides a significant improvement in impact strength and flexibility over s.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9364 XAP² ™ POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9364 XAP2 ™ is highly impact modified grade for demanding applications. Hostaform® S 9364 XAP2 ™ provides a significant improvement in impact strength and fl.. |
|||
Die Temperature | 180 - 195 °C | 356 - 383 °F | Extrusion Molding |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | Extrusion |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | Extrusion |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL0521 High Density Polyethylene BL0521 is a high molecular weight (HMW), high density polyethylene. The main properties are: good impact resistance, high stiffness, very good stress crack resistance. Applications: cans and drums .. |
|||
Die Temperature | 180 °C | 356 °F | |
Lubrizol Estane® ZHF 78AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 78AT0 NAT021 is a soft, polyether based, NHFR thermoplastic polyurethane (TPU) compound.Features: Soft, transparent, flame retardant.Uses: Wire and CableAvailable in Europe, Middl.. |
|||
Die Temperature | 180 °C | 356 °F | 6, Zone 1, Extrusion |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Die Temperature | 180 °C | 356 °F | Blown film |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Die Temperature | 180 °C | 356 °F | Blown film |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Die Temperature | 180 °C | 356 °F | Blown film |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Die Temperature | 180 °C | 356 °F | 6, Zone 1, Extrusion |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Die Temperature | 180 °C | 356 °F | Extrusion |
Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane Type: Estane® ALR CL87A is an aliphatic, polycaprolactone-based TPU with a Shore A Durometer of 85-90.Features: Contains a UV package that enhances outdoor weatherability. This high performance re.. |
|||
Die Temperature | 180 °C | 356 °F | 6, Zone 1, Extrusion |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Die Temperature | 180 °C | 356 °F | Zone 2, Extrusion |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Die Temperature | 180 °C | 356 °F | Blow Film |
DuPont Appeel® LSR11D554 Lidding Sealant Resin Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to poly.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Elastron® G SEBS Elastomer Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v.. |
|||
Die Temperature | 180 - 210 °C | 356 - 410 °F | |
Elastron® TPO Elastomer wide hardness rangedoes not require vulcanization-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with very low conduct.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1442E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 180 - 210 °C | 356 - 410 °F | |
Celanese Hostaform® MR130HPB POM, Specialty Preliminary Data SheetInformation provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9362 POM, Impact Modified Hostaform« acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform« S 9362 provides good impact strength while improving modulus and weld .. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified Preliminary Data SheetInformation provided by Celanese |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9364 XAP² ™ POM, Impact Modified Hostaform« acetal copolymer grade S 9364 XAP2 Ö is highly impact modified grade for demanding applications. Hostaform« S 9364 XAP2 Ö provides a significant improvement in impact strength and fl.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Celcon® MR25B POM, Specialty
(Unverified Data**) Celcon® MR25B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.improved media resistance, improved toughnessStandard reciprocating screw injectio.. |
|||
Die Temperature | 180 - 290 °C | 356 - 554 °F | Average value: 240 °C Grade Count:9 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an.. |
|||
Die Temperature | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® C 36021 POM, Unfilled Hostaform« C 36021 is an unfilled acetal copolymer grade formulated for high flow while retaining a good balance of mechanical properties.Information provided by Celanese |