Thermal Properties Metric English Comments
Melting Point 94.0 °C
201 °F
Exxon Method
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e..
Melting Point 94.0 °C
201 °F
Upon Melting via DSC/ASTM D3418
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin  (discontinued **)
Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly..
Melting Point 94.0 °C
201 °F
Upon Melting via DSC/ASTM D3418
DuPont Bynel® 1E554 Modified EVA Adhesive Resin  (discontinued **)
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Melting Point 94.0 °C
201 °F
DSC; ASTM D3418
DuPont™ Surlyn® 1605SBR Sodium Ionomer Resin for Extrusion Coating  (discontinued **)
Surlyn® 1605SBR is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceuti..
Melting Point 94.0 °C
201 °F
DSC; ASTM D3418
DuPont™ Surlyn® 1702-1 Zinc Ionomer Resin for Extrusion Coating  (discontinued **)
Surlyn® 1702-1 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutic..
Melting Point 94.0 °C
201 °F
10°C/min; ASTM D3418
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical
Melting Point 94.0 °C
201 °F
10°C/min; ASTM D3418
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical
Melting Point 94.0 °C
201 °F
Freezing Point via DSC/ASTM D3418
DuPont 20 Series 20-6064 Specialty Polyethylene Resin
DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding..
Melting Point 94.0 °C
201 °F
By DSC; ASTM D3418 - ISO 3146
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It..
Melting Point 94.0 °C
201 °F
TRN-14
Tipco Tipcolite® TPF 1211 - Unreinforced Phenolic Resin having 53 mm Norton Flow with 12% Hexamine
Unreinforced Phenolic Resin having 53mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: Grinding WheelsInformation provided by the Manufacturer, Tipco Industries Ltd., In..
Melting Point 94.0 °C
201 °F
Peak DSC; ASTM D-3418
Westlake EB502 12.5% EVA Copolymer
Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea..
Melting Point 94.0 °C
201 °F
DSC Peak; D3418
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength m..
Melting Point 94.0 °C
201 °F
DSC; ASTM-D3418
Westlake EF532 12% EVA Copolymer (Experimental Product)
Westlake EF532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low seal initiation temperature, excel..
Melting Point 94.0 °C
201 °F
ASTM D3418
Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer
Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low ..
Melting Point 94.0 °C
201 °F
DSC; ASTM D3418
DuPont Appeel® LSR20D751 Lidding Sealant Resin
Appeel® LSR20D751 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu..
Melting Point 94.0 °C
201 °F
By DSC; ASTM D3418 - ISO 3146
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Melting Point 93.9 °C
201 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® LD 705.MJ Molding, extrusion and compounding resin
Escorene Ultra LD 705.MJ is a fraction melt index, 13.3 wt% vinyl acetate copolymer suitable for use in making blow molded articles, extruded profiles and compounds.Information provided by ExxonMobi..
Melting Point 93.9 °C
201 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil EXACT™ 3131 Plastomer for Cast Film Applications
Product Description: Exact 3131 is an ethylene-based hexen plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3131 is designed for both monolayer and multilayer coex..
Melting Point 94.0 °C
201 °F
ASTM D3418, ISO 3146
DuPont™ Appeel® 72D727 Sealing Resin
DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Melting Point 94.0 °C
201 °F
ASTM D3418, ISO 3146
DuPont™ Appeel® 72D799 Sealing Resin
DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Melting Point 94.0 °C
201 °F
ASTM D3418, ISO 3146
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
Melting Point 94.0 °C
201 °F
ASTM D3418, ISO 3146
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Melting Point 94.0 °C
201 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® A560 Polymer Modifier
DuPont™ Fusabond® A560 is a chemically modified ethylene acrylate copolymer Used as a polymer modifier
Melting Point 94.0 °C
201 °F
DSC
DuPont™ Surlyn® 8940 Ionomer Resin, Sodium
Surlyn® 8940 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
Melting Point 94.0 °C
201 °F
DSC, 10°C/min; DuPont Test
Dow Engage® 8440 Polyolefin Elastomer
Description: Engage® 8440 polyolefin elastomer is an ethyleneoctene copolymer that performs well in a wide range of thermoplastic elastomer applications. It is an excellent thermoplastic elastomer ..
Melting Point 94.0 °C
201 °F
ASTM-D3418
Braskem TN2005 EVA General Film Copolymer
TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e..
Melting Point 94.0 °C
201 °F
BASF Lucalen® A 2710 H Ethylene/Acrylate Copolymer
Product with properties which are typical of flexible PVC and of low density polyethylene. Suitable for flexible pipes, profiles and seals.Data was collected by ISO methods and provided by BASF.
Melting Point 94.0 °C
201 °F
DSC; ASTM D3418
DuPont Appeel® LSR11D625 Lidding Sealant Resin  (discontinued **)