Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 482 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 2401 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2401 MT Natural is an unreinforced, high molecular weight PBT that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Maste..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese Celanex® 3316 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3316 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/16 inch), 30% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechan..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4300FC PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 4300FC is a toughened, 30% glass reinforced PBT for use in food contact applications.30% glass reinforced PBT for use in food contact applicationsInformation provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® MT2008 PBT  (Unverified Data**)
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Unfilled PBT for medical ..
Die Temperature 250 °C
482 °F
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)  (Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
Die Temperature 250 °C
482 °F
For high temperature coextrusions.
DuPont Bynel® 41E687 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Die Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer
Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Die Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer
Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also..
Die Temperature 250 °C
482 °F
Cast film
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va..
Die Temperature 250 - 290 °C
482 - 554 °F
Cast Film Extrusion
Braskem PB681 LDPE Cast and Blown Film Extrusion, Injection Molding Polyethylene
PB681 is a resin produced under high pressure in a tubular reactor. This resin presents excellent 'draw down' (stability to form fine films). The films produced with this resin have excellent optica..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1400FC PBT, Unfilled
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1462Z PBT, 30% Glass Reinforced
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 1600FC PBT, Unfilled
Celanex 1600FC is a high molecular weight grade of unreinforced polybutylene terephthalate for use in food contact applications that can be used in both extrusion and injection molding applications...
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 2000-3FC PBT, Unfilled
Celanex 2000-3FC is a general purpose, unreinforced PBT with a good balance of mechanical properties and processabillity for use in food contact applications.. Celanex 2000-3FC is a high flow mater..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 2001 PBT, Unfilled
Celanex 2001 is an unreinforced polybutylene terephthalate resin with improved hydrolysis resistance developed for use in fiber optic buffer tube applications. Celanex 2001 exhibits the high melt st..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese CELANEX 2016 PBT, Unfilled
Celanex 2016 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), unreinforced polybutylene terephthalate which has an excellent balance of mechanical propertie..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 3100-2 PBT, 7.5% Glass Reinforced
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.Information ..
Die Temperature 250 - 255 °C
482 - 491 °F
Celanese CELANEX 3216 PBT, 15% Glass Reinforced
Celanex 3216 is a non-exuding (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch ),15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties ..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 3300LM PBT, 30% Glass Reinforced
Celanex 3300LM is a 30% glass reinforced lasermarkable grade specially formulated to yield crisp marks when subjected to a Nd:YAG laser or equivalent operated at 1064nm or 532nm. Lasers operating i..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX MT2008 PBT, Unfilled
Celanex MT2008 is a medical grade unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by C..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3300HR PBT, 30% Glass Reinforced
Celanex 3300HR is a 30% glass reinforced polybutylene terephthalate which has excellent hydrolysis resistance, mechanical properties and processabilityTo avoid hydrolytic degradation during processi..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 4305 PBT, 33% Glass Reinforced
Celanex 4305 is a 33% glass reinforced, toughened, thermoplastic polyester.To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less tha..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 2500 PBT, Unfilled
Chemical abbreviation according to ISO 1043-1: PBTInformation provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 531HS PBT, Glass Reinforced
Celanex 531HS is a 30% fiberglass reinforced PBT which has an excellent balance of mechanical properties and processability. Celanex 531HS is specifically designed to exhibit excellent thermal shoc..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3200HR PBT, 15% Glass Reinforced
Celanex 3200HR is a 15% glass filled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processability.To avoid hydrolytic degradation during processi..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 3209HRT PBT, 15% Specialty
Celanex 3209HRT is a non-lubricated, 15% fiberglass reinforced Polybutylene Terphthalate material that has excellent hydrolysis resistance, toughness and improved flow.Information provided by Celane..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1400FC PBT  (Unverified Data**)
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese CELANEX 4302 PBT, 30% Glass Reinforced
Celanex 4302 is a 30% glass reinforced PBT designed for improved mold flow, warp resistance and surface appearance.Information provided by Celanese
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese Corporation.
Die Temperature 250 - 260 °C
482 - 500 °F
Celanese Celanex® 6035GB20 PBT, 20% Glass Bead Filled
20% glass bead filled PBT.Information provided by Celanese Corporation.
Copyright © lookpolymers.com All Rights Reserved