Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 160 - 199 °C | 320 - 390 °F | |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Middle Barrel Temperature | 160 - 199 °C | 320 - 390 °F | |
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex.. |
|||
Middle Barrel Temperature | 160 - 199 °C | 320 - 390 °F | |
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Middle Barrel Temperature | 160 - 199 °C | 320 - 390 °F | |
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Middle Barrel Temperature | 160 - 199 °C | 320 - 390 °F | |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Middle Barrel Temperature | 160 - 199 °C | 320 - 390 °F | |
PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - .. |
|||
Middle Barrel Temperature | 160 - 171 °C | 320 - 340 °F | |
Kleerdex Kydex® P51 Acrylic/PVC Extrusion Compound
(discontinued **) Profile extrusion compound for building productsApplications: Handrails, crashrails, bumper guards, corner guardsFeatures: Extruded profiles made with P51 are extremely resistant to harsh chemicals .. |
|||
Middle Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
Kleerdex Kydex® P90 Acrylic/PVC Extrusion Compound
(discontinued **) Low heat release aviation gradeApplications: Kydex P90 is designed for extrusion of profiles which need to meet the highest flammability requirement of PAR 25.853a for vertical burn, rate of heat re.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | |
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Transition, Extrusion |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Transition, Extrusion |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Transition, Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
Stellarchem MP-845B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce.. |
|||
Middle Barrel Temperature | 160 - 200 °C | 320 - 392 °F | |
Unitika TERRAMAC TP-4000 Polylactic Acid (PLA) Basic grade, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 160 - 200 °C | 320 - 392 °F | |
Unitika TERRAMAC TP-4030 Polylactic Acid (PLA) Soft, Extrusion, blow, and foam sheet grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 160 °C | 320 °F | Blown film |
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |