Samsung Cheil Industries Infino® HI-1001BG PC/ABS, Metal Plating Grade

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® HI-1001BG PC/ABS, Metal Plating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PC/ABS material that can be used in automobile wheel cap and air-conditioner panelInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 63.6 g/10 min

@Load 10.0 kg,
Temperature 250 °C
63.6 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 48.1 MPa
6970 psi
50 mm/min; ASTM D638
Flexural Strength 73.5 MPa
10700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 4.22 J/cm

@Thickness 3.17 mm
7.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C

@Thickness 6.40 mm
198 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 106 °C
223 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 - 6.00 mm
HB

@Thickness 0.0591 - 0.236 in