Material Notes:
DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look more like true, clear engineered plastic. In addition, WaterShed XC has been formulated with the DSM Somos Oxetane Advantage™ - an advanced chemistry platform that produces parts with outstanding water resistance and high dimensional stability.ApplicationWaterShed XC 11122 offers many properties that mimic traditional engineering plastics including ABS and PBT. This makes the material ideal for many applications in the automotive, medical and consumer electronics markets and include:LensesPackagingWater flow analysisRTV patternsDurable concept modelsWind tunnel testingQuickcast patternsInformation Provided by DSM Desotech Inc.
Physical Properties Metric English Comments
Density 1.12 g/cc

@Temperature 25.0 °C
0.0405 lb/in³

@Temperature 77.0 °F
Water Absorption 0.35 %
0.35 %
ASTM D570-98
Viscosity 260 cP

@Temperature 30.0 °C
260 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.1 - 53.6 MPa
6830 - 7770 psi
ASTM D638M
Elongation at Break 11 - 20 %
11 - 20 %
ASTM D638M
Elongation at Yield 3.3 - 3.5 %
3.3 - 3.5 %
ASTM D638M
Modulus of Elasticity 2.65 - 2.88 GPa
384 - 418 ksi
ASTM D638M
Flexural Strength 63.1 - 74.2 MPa
9150 - 10800 psi
ASTM D790M
Flexural Modulus 2.04 - 2.37 GPa
296 - 344 ksi
ASTM D790M
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256A
Graves Tear Strength 150.3 kN/m
857.5 pli
ASTM D1004
Thermal Properties Metric English Comments
CTE, linear 66.0 - 67.0 µm/m-°C

@Temperature -40.0 - 0.000 °C
36.7 - 37.2 µin/in-°F

@Temperature -40.0 - 32.0 °F
ASTM E831-00
90.0 - 96.0 µm/m-°C

@Temperature 0.000 - 50.0 °C
50.0 - 53.3 µin/in-°F

@Temperature 32.0 - 122 °F
ASTM E831-00
170 - 189 µm/m-°C

@Temperature 50.0 - 100 °C
94.4 - 105 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
185 - 189 µm/m-°C

@Temperature 100 - 150 °C
103 - 105 µin/in-°F

@Temperature 212 - 302 °F
ASTM E831-00
Deflection Temperature at 0.46 MPa (66 psi) 45.9 - 54.5 °C
115 - 130 °F
ASTM D648-98c
Deflection Temperature at 1.8 MPa (264 psi) 49.0 - 49.7 °C
120 - 121 °F
ASTM D648-98c
Glass Transition Temp, Tg 39.0 - 46.0 °C
102 - 115 °F
ASTM E1545-00
Optical Properties Metric English Comments
Refractive Index 1.512 - 1.515
1.512 - 1.515
ASTM D542
Electrical Properties Metric English Comments
Dielectric Constant 3.4 - 3.5

@Frequency 1.00e+6 Hz
3.4 - 3.5

@Frequency 1.00e+6 Hz
ASTM D150-98
3.7 - 3.9

@Frequency 1000 Hz
3.7 - 3.9

@Frequency 1000 Hz
ASTM D150-98
3.9 - 4.1

@Frequency 60.0 Hz
3.9 - 4.1

@Frequency 60.0 Hz
ASTM D150-98
Dielectric Strength 15.4 - 16.3 kV/mm
391 - 414 kV/in
ASTM D149-97a
Descriptive Properties Value Comments
Appearance Optically Clear
Dp (mm) 0.16
Slope of cure-depth vs. ln(E) curve
E10 (mJ/cm2) 54
Exposure that gives 0.254mm thickness
Ec (mJ/cm2) 11.5
Critical exposure