Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murylon® 6 Cast Nylon 6 Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.Specia.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
|
Murtfeldt Murylon® B Nylon 6 Murylon® B natural has the best impact resistance of all Murylon materials. This material is especially suited for use in machine construction thanks to an excellent combination of mechanical prope.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 23.0 - 100 °C |
50.0 µin/in-°F @Temperature 73.4 - 212 °F |
|
Murtfeldt Murylon® HT Nylon 46 The use of this highly temperature resistant polyamide enables reliable operation up to a constant service temperature of 155°C . The material retains its rigidity and creep strength over the entir.. |
|||
CTE, linear | 90.0 - 160 µm/m-°C @Temperature 25.0 - 200 °C |
50.0 - 88.9 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
CTE, linear | 90.0 - 110 µm/m-°C @Temperature 25.0 - 200 °C |
50.0 - 61.1 µin/in-°F @Temperature 77.0 - 392 °F |
ASTM D696 |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
CTE, linear | 90.0 - 96.0 µm/m-°C @Temperature 0.000 - 50.0 °C |
50.0 - 53.3 µin/in-°F @Temperature 32.0 - 122 °F |
ASTM E831-00 |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature >=143 °C |
50.0 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature >=143 °C |
50.0 µin/in-°F @Temperature >=289 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature >=152 °C |
50.0 µin/in-°F @Temperature >=306 °F |
Average above Tg; ISO 11359 |
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 93.3 - 238 °C |
50.0 µin/in-°F @Temperature 200 - 460 °F |
ASTM D696 |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature -20.0 °C |
50.0 µin/in-°F @Temperature -4.00 °F |
ASTM D696 |
Micropol Isoplas P501 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
CTE, linear | 90.0 µm/m-°C @Temperature -20.0 °C |
50.0 µin/in-°F @Temperature -4.00 °F |
ASTM D696 |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
CTE, linear | 90.0 µm/m-°C @Temperature -20.0 °C |
50.0 µin/in-°F @Temperature -4.00 °F |
ASTM D696 |
Borealis BorPEX™ HE2515 High Density Polyethylene Compound for Silane Crosslinked Pipes BorPEX HE2515 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for flexible cr.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature <=150 °C |
50.0 µin/in-°F @Temperature <=302 °F |
ISO E 831 |
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature -20.0 °C |
50.0 µin/in-°F @Temperature -4.00 °F |
ASTM D696 |
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane)) BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkab.. |
|||
CTE, linear | 90.0 - 96.0 µm/m-°C @Temperature 0.000 - 50.0 °C |
50.0 - 53.3 µin/in-°F @Temperature 32.0 - 122 °F |
UV Postcure; ASTM E831-05 |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
CTE, linear | 90.0 - 95.7 µm/m-°C @Temperature 100 - 150 °C |
50.0 - 53.2 µin/in-°F @Temperature 212 - 302 °F |
ASTM E831-00 |
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure DescriptionNanoTool produces strong, stiff, high temperature resistant composite parts on conventional stereolithography machines. This third generation of Somos® ProtoComposite materials is heavi.. |
|||
CTE, linear | 90.0 - 96.0 µm/m-°C @Temperature 0.000 - 50.0 °C |
50.0 - 53.3 µin/in-°F @Temperature 32.0 - 122 °F |
ASTM E831-00 |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
CTE, linear | 90.0 µm/m-°C @Temperature 500 °C |
50.0 µin/in-°F @Temperature 932 °F |
|
Dow SiLK™ D Semiconductor Dielectric Resin SiLK™ D resin provides a more controlled coefficient of thermal expansion (CTE) profile at elevated temperatures as compared to earlier versions of SiLK™ resin.Information provided by Dow |